Bright yellow plastic wedge leaning in a corner, resting against the junction of two wooden surfaces. A narrow grey strip runs along the seam where the wood panels meet.

Bonding with Epoxy Fillets

By Tom Pawlak — GBI Technical Advisor

Building with epoxy fillets is especially beneficial when attaching bulkheads to hull sides, attaching hull sides to hull bottoms where the faces of the plywood are coming together at ever-changing angles. Gluing plywood structures together with epoxy fillets saves considerable time constructing the joints and reduces the overall weight of the structure compared to more traditional methods using wooden cleats and screws. The strength and gap-filling qualities of epoxy eliminate the need for precisely fitted wood cleats that otherwise require time and skill to create. When gluing with conventional adhesives, that are non-gap filling such as resorcinol glue, wood cleats need to be well fitted, need to be wide enough to provide sufficient glued surface area, and provide enough thickness for screws to be driven into.

Because epoxy can be thickened with high-density fillers into a non-slumping consistency it can bridge large gaps in wood joints, without loss of strength, thus saving a great deal of time labor otherwise needed to create a strong joint.

Central vertical plate on a base, with curved fillets around it showing density contrast: left Low-Density Fillet, right High-Density Fillet. Low-Density Fillet High-Density Fillet
Cross-section of low-density and high-density epoxy fillets. Low-density fillets require a much larger radius than high-density fillets to make joints of the same strength.

A fillet is a continuous bead of thickened epoxy mixture applied to the angle created between two parts. It increases the surface area of the bond and serves as a structural adhesive and brace.

Filleting creates an effective glue joint that requires no fasteners of any kind and can result in a joint that is as strong as the parts being joined together.

Object: instructional diagram titled 'How to apply a fillet' showing a joint coated with epoxy. Action: coat/join parts, shape fillet, and remove excess epoxy. Context: woodworking with a mixing stick. Transcription of visible text: How to apply a fillet 1. Coat and join the parts 2. Apply and shape the fillet 3. Clean away excess epoxy outside of the fillet Joint coated with epoxy and temporarily held with staples 804 Mixing Stick Excess Tangent point of mixing stick produces a clean margin area that aids in the cleanup of excess epoxy mixture
How to apply an epoxy fillet: 1. coat and join the parts. 2. Apply and shape the fillet. 3. clean away excess epoxy outside the fillet.

If wood components have not previously been sealed in epoxy, it is good practice to apply a thin coat of epoxy to saturate the surface prior to applying the thickened epoxy fillet so the edges of the fillet don’t soak into the dry wood and cause a dry edge.

You can let the initial coat of epoxy cure, then sand it in preparation for applying the fillet; or you can allow the initial coat of epoxy to tack up a bit before applying the thick epoxy fillet; or you can wipe off uncured epoxy remaining on the surface with a paper towel so the uncured epoxy does not cause the thickened epoxy to slide or slump. In this last scenario, by wiping off the remaining liquid uncured epoxy from the surface you can now apply the thickened epoxy fillet without it sliding off of the wet and uncured liquid epoxy.

Object: a guide on fillet sizes for wood joints. Action: shows low- and high-density fillets under load, with diagrams and a table of thickness vs. fillet radius for failure modes. Transcription (text legible): - Determining fillet size - Fillet size depends on whether you are using low-density (less strong/less dense thickener) or high-density fillets (stronger/denser thickened). The chart shows the recommended radius size for fillets. Experiment to find the proper materials you are using. - Plywood Thickness Fillet Radius - High-density Fillets - Low-density Fillets - Low-Density Fillet 1. Low-density fillet compresses under load. 2. Fillet fails in tension and wood failure along grain. 3. Wood failure along the base of the joint. - High-Density Fillet Load Experimentation with the fillet can produce a joint that will fail under load. Failure mode for a properly sized fillet: wood failure. Unreadable/noisy segments: - Specific table values under Plywood Thickness and Fillet Radius (not legible) - Some wording on the right panel’s caption/notes (not legible)

An epoxy fillet can be especially effective when joining parts that meet at difficult angles like where bulkheads meet the hull sides near the bow. Other instances would be where plywood hull sides meet the hull bottom or chine, where hull sides meet at the bow and where hull sides join the deck at the sheer. Historically these joints required well-fitted pieces of wood that the plywood could be glued and screwed into.

Applications where fillets are common and helpful:

Stitch and glue boatbuilding

Gluing plywood structures with epoxy fillets has become extremely popular because it allows extremely thin plywood panels to be bent into compound curves and temporarily stitched together at varying angles with plastic wire ties or copper wire that are then permanently joined together with epoxy fillets.

More often than not, these fillets along the chine and at the bow and stern are fiberglassed to provide fiber reinforcement over what would otherwise be a butt-glued joint. Once the fiberglass is applied and cured, the joints are amazingly resilient and strong.

Gluing stringers and frames into hulls

Fillets are also used when gluing stringers and frames into hulls. In these applications, fiberglass fabric (called tabbing) is often applied over the fillet that extends and onto the hull and stringer 2-3” to reinforce the joint. Smooth rounded fillets bridge the hard corner and give the fiberglass reinforcement something to be attached to. Without the fillet, fiberglass fabric won’t go into a square corner well, and the strength would be decreased.

Two yellow rectangular tags with holes lie on a white backdrop; a blue rod with white spheres at each end stands upright between two clear spoons, forming a toy-like arrangement.
A wide variety of objects can be used to make fillets. Plastic spoons and rounded off 808 Plastic Spreaders can be particularly useful.

Color-Matched Fillets

When hull interiors are to be finished natural, epoxy fillets are often colored with a blend of thickeners to achieve colors that match the natural color of wood.

One way to achieve a natural brown fillet would be to use our 405 Filleting Blend filler. It is a blend of dry powder fillers designed to produce medium brown thickened epoxy.

You can also make your own color-matched fillets. Some people use sanding dust, taken from their palm sander dust pickup bag after sanding the wood that they are trying to match. If you use sanding dust exclusively however to thicken the epoxy, it will be grainy to work with and it will be significantly darker than the original wood that it was created from.

A better approach is to initially thicken a batch of epoxy with 406 Colloidal Silica filler to a mayonnaise consistency (this will create a translucent white/smooth and creamy epoxy) then add wood sanding dust until you arrive at a color you are happy with. The translucent white color of the 406 filler is easily overcome by the wood sanding dust. Add a little wood sanding dust and you’ll get a colored epoxy that is lighter than the wood. Add a lot of the wood sanding dust to the 406 filler thickened epoxy mix and it will become dark. See the photos of three different wood types with four dollops of thickened epoxy on each.

You will discover that if the 406 filler is used to thicken the epoxy alone it gives the mix a translucent white look that will nicely offset the darkening effect of wet wood flour (sanding dust) allowing you to arrive at a color that perfectly matches the wood tone. To do this well though, you will need to have a varnished wood surface or an epoxy-coated surface to see what the wood looks like as you try to color match the thickened epoxy for making fillets. What the epoxy looks like while uncured is what it will look like after it cures.

So, if a natural wood finish is desired, you can add to the overall beauty and elegance of a glued plywood structure by using color-matched epoxy fillets.

Five crescent-shaped slabs, from white to dark brown, are arranged in three horizontal rows on wood and a dark surface. Small powdery piles sit to the right of each row.
Three different wood types with four dollops of thickened epoxy on each. The first dollop (white on the far left of each) is thickened with all 406 Colloidal Silica filler. The second one is thickened with 406 filler and a bit of wood sanding dust. The third one is thickened with 406 filler then thickened with significantly more wood sanding dust. The fourth one is thickened with wood sanding dust exclusively and is by far the darkest of them all. The dry sanding dust of each wood type is set next to the last thickened epoxy dollop.

The illustrations in this article are taken from The Gougeon Brothers on Boat Construction pages 102 and 103.