Tips for mixing small batches of epoxy By Tom Pawlak — GBI Technical Advisor My favorite way to mix small batches of WEST SYSTEM® Epoxy, when less than full pump strokes on the mini pumps are required, is by metering resin and hardener into a graduated cylinder made with a plastic syringe. The 807 Plastic Syringes, […]