by Jim Derck—GBI Technical Advisor It’s difficult to prevent cloth from lifting when fiberglassing around a sharp wooden corner. Even if you were able to lay glass tightly around a sharp corner, it could easily be dented. The slightest compression of the underlying wood could leave a void, and an invitation for moisture and the […]