An upright West System G/flex thickened epoxy adhesive tube in a clear blister pack on a white-blue retail card. Transcribed text on packaging: - WEST SYSTEM - G/flex - THICKENED EPOXY ADHESIVE - ÉPAISSI ÉPOXYDE - For tough permanent, waterproof repairs on plastics - CAUTION / ATTENTION - IRRITANT - Read cautions on back panel / Lire les cautions au dos du panneau - .42 fl oz / 12.5 ml - Resin / Résine - Hardener / Durcisseur

G/flex® 655 Epoxy

Now in a Convenient Dual Syringe

Versatile G/flex Thickened Epoxy Adhesive is now available in a dual syringe for convenient dispensing. The G/flex 655-1 syringe contains 0.42 oz. of resin and 0.42 oz. of hardener, the perfect amount to keep on hand for small repair jobs. Depressing the plunger on the dual syringe dispenses the proper 1:1 ratio of G/flex resin and hardener.

This new product became available through West System® retailers on January 1, 2021.

G/flex 655 is a 2-part, pre-thickened epoxy system that bonds tenaciously to plastics including HDPE, LDPE, ABS, PVC, Polycarbonate, and Hypalon. Its viscosity is similar to gel toothpaste so it won’t run or sag, even on vertical surfaces. The G/flex 655-1 dual syringe allows users to dispense the epoxy in very small quantities, providing big strength for little repairs.

This toughened epoxy makes permanent, waterproof structural bonds. It absorbs the stresses of expansion, contraction, shock, and vibration. In addition to its effectiveness in adhering to plastics, this formulation is also excellent for bonding metal, glass, masonry, and fiberglass. It even works great on typically hard-to-bond substrates including dense, oily, or damp wood varieties.

We introduced G/flex in our WEST SYSTEM product line in 2008 and this versatile epoxy has been popular among epoxy users ever since.

G/flex 655 comes in a wide variety of sizes; the 655-1 dual syringe is the smallest. To learn more about G/flex epoxy, visit westsystem.com.