Object: a vintage phonograph with a large black horn attached to a wooden cabinet. Action: it sits idle on display. Context: indoors, wood-paneled walls, a white placard nearby (text illegible).

Repairing an Edison Concert Phonograph

By Tom Pawlak — GBI Technical Advisor

Ronnie Janowicz, a good friend of mine, called to say the wooden horn on his antique Edison Concert phonograph was cracked. I had Ronnie bring it by so I could take a look.

I told him it could be repaired very nicely with epoxy if that is what he wanted to do. “Why wouldn’t I want it repaired that way?” he asked. I explained that repairing an antique with epoxy may affect its resale value if the potential purchaser objects to the repair. Some collectors take a dim view of wooden antiques being repaired with epoxy because repairs are not easily reversible like they would be if hide glue was used for repair instead.

Ronnie said he had more confidence with the epoxy and was not worried about potential devaluation because the phonograph would stay in his family for at least another generation.

Leather strap, curved and reddish-brown, shows a long crack along its center. The edge looks darker and frayed. The blurred background suggests an indoor workshop or shop.

I told him I would be happy to repair it in a very non-invasive way and if I did my job of repair well, he would not be able to tell that it had been repaired.

I gathered the following items before starting the job:

  • Spring clamps
  • Shop light with an incandescent bulb
  • 807 Plastic Syringe
  • G/flex 650 Epoxy
  • Small plastic tarp
  • Cheese cloth

I warmed the damaged section of the horn by placing a shop light close by for 15 minutes or so. I had to be careful because it is easy to damage the finish/patina on the surface of wooden antiques with just a bit too much heat.

An orange-brown copper curved metal surface is held by a metal clamp at a joint. The scene is a workshop with tools, tape, and miscellaneous equipment visible in the background. Text in image: The label on the right side contains small, blurry lettering and is not legible.

I mixed a small batch of G/flex 650 and transferred it into an 807 Plastic Syringe.

I removed the heat source just before applying a bead of G/flex 650 Epoxy along the crack with the tip of the plastic syringe. Because the wood was warm (maybe 125°F) the epoxy thinned on contact and easily soaked into the cracked section. I applied epoxy multiple times over several minutes to fill any remaining voids in the joint.

Epoxy applied to the crack through a syringe.

When the joint would not absorb any more epoxy, I clamped the area with spring clamps, allowed the excess to squeeze out, wiped off most of the excess with white paper towels and wiped off the last of the epoxy smears with dry cheesecloth.

Close-up shows a black glossy panel clamped by two greenish, rusted metal arms; a red textured edge lies nearby, with a cluttered workshop blurred in the background.

I wanted to avoid using any solvent for cleanup because these old finishes are easily damaged with solvent. I have used dry cheesecloth to remove the last slight smudges of uncured epoxy from the surrounding area many times before with excellent results. An old terrycloth towel will work just as well.

IMG_6905

I allowed the epoxy to cure overnight then applied a bit of Old English® furniture polish to the horn with cheese cloth.

An antique gramophone with a large black horn sits on a wooden dresser; a white paper note hangs from the front, in a room with wooden panel walls.

I think from the photos you’ll agree that the repair came off fine. More importantly, Ronnie is happy. He sent this photo of the Edison with horn installed along with the original bill of sale from March 18, 1913.