Are you the kind of person who just can’t get enough of a good thing? Looking for a better way to squeeze out that last little bit of G/flex 655 Thickened Epoxy Adhesive from your tube rather than resorting to pliers, a vise, or maybe even Grandma’s rolling pin? Maybe you’d like to get a fatter bead of adhesive or your tube is a bit clogged. Boy, do we have some easy and inexpensive tricks for you!

Cut a 4" long slot through the center of the PVC pipe. Insert the crimped end of the G/flex tube through both horizontal cuts in the PVC pipe. For added "G/flex appeal" add a PVC cap. Take hold of the handle and you're now ready to roll G/flex out of the tube

Question:

“I love your G/flex adhesive! Do you have any nifty tips on squeezing the last little bit of adhesive out of the tube with ease?”

Useful and Inexpensive Trick:

Not long ago this very subject was the topic of discussion that came up between J.R. Watson and me. Squeezing in a bit of shopping on my lunch, it just so happened that I found myself face-to-face with a display of toothpaste squeezers. On my way back to work I felt as though I had just solved all the world’s problems. Perfect! Or so I thought. Although the concept was good, the little toothpaste squeezer just didn’t stand a chance next to the rigid metal G/flex tube. However, it did give the innovative J.R. Watson an idea. Using very little time and effort, we whipped up this very cool gadget making it a snap to squeeze out the last drop of adhesive.

Here’s what you’ll need:

1/2″ diameter PVC pipe

1 PVC cap to fit the 1/2″ pipe

Here’s what you’ll need to do:

You will obviously need to make two, one for the resin tube and one for the harder. But for simplicity’s sake, we’ll just show one tube being created.

Cut the 1/2″ diameter pipe to approximately 7″ long. The additional length creates an easily gripped handle. So, for you extra- large-handed men, petite-handed women, or vice/versa, cut to length accordingly.

  1. Cut a 4″ long slot through the center of the tube.
  2. Insert the crimped end of the tube through both horizontal cuts.
  3. For added ‘G/flex’ appeal add a PVC cap.
  4. Take hold of the handle and you are now ready to roll.

Question

“I’d like a bit more of the adhesive to squeeze out of my G/flex tube, got any tips? By the way, your stuff rocks!”

Useful and Inexpensive Tip:

Simply poke the sharpened end of a pencil into the open tip, applying enough pressure to increase the diameter of the hole. It’s cheap, easy, and works like a charm. The amount of adhesive that comes out of the tube afterward can double in volume, depending on how far the pencil is inserted.